Line 24: | Line 24: | ||
* Designed Gd<sub>2</sub>O<sub>3</sub> powder holder for CaGaS Phase II. | * Designed Gd<sub>2</sub>O<sub>3</sub> powder holder for CaGaS Phase II. | ||
** Have spray on clear coat to seal plastic after printing is complete. | ** Have spray on clear coat to seal plastic after printing is complete. | ||
+ | |||
+ | * Continued to research live time correction for HPGe count rates and ''think'' I have applied the correction correctly at the initial measurement level, which will be propagated through to efficiency calculations. | ||
+ | |||
+ | * Researched and tested different integration methods for more accurate measurement of counts in energy peak to compare to Gaussian fit. | ||
='''Previous Page'''= | ='''Previous Page'''= | ||
[[PAS Experiment]] | [[PAS Experiment]] |
Revision as of 17:36, 29 September 2022
09/19/22
- Investigated non-linearity of peak sensing ADC due to issues arising in energy calibrations and efficiency measurements.
- Modified existing calibration code to use non-linear regression to account for ADC.
- Sourced material needed for CaGaS Phase II setup.
- Calculated ADC dead time for live-time correction to efficiency measurement count rates and calculated dead time per experiment.
- Designed holder for Gd foils needed for CaGaS Phase II experiment. To be 3D printed and tested for tolerances.
09/26/22
- Printed both parts of the Gd foil holder for CaGaS Phase II.
- Parts fit together more than adequately considering they're 3D printed and not machined.
- M3 bolts threaded through first part of the holder.
- M3 nuts press fitted into the second part of the holder.
- Edited rebinning code for energy calibrations for data sets collected with ADC to account for changes in calibration code.
- Energy calibration script now uses 2nd order polynomial regression to account for nonlinearity of ADC
- The coefficients from the regression are passed to another script to rebin ADC data from channel to energy, preserving bin count, but bin width will increase as a function of energy.
- Designed Gd2O3 powder holder for CaGaS Phase II.
- Have spray on clear coat to seal plastic after printing is complete.
- Continued to research live time correction for HPGe count rates and think I have applied the correction correctly at the initial measurement level, which will be propagated through to efficiency calculations.
- Researched and tested different integration methods for more accurate measurement of counts in energy peak to compare to Gaussian fit.